Properties:
* A low-carbon version of N02200
* Low hardness and lower work-hardening rate
Applications:
* Good for spinning and cold forming.
* Comparing with N02200, N02201 has a better corrosive resistance. It is more suitable than N02200 while exposing at temperature above 600°F (315°C).
* Can be used for crucibles having capable of withstanding up to 2000°F (1100°C) in normal oxidation condition
* Typical applications are used for caustic evaporators, combustion boats, electroplating bars, and some electronic components.
Chemical Composition %
Grade | UNS | Chemical,% | ||||||
C | Si | S | Mn | Ni | Fe | Cu | ||
Nickel 201 | N02201 | 0.02 max | 0.35 max | 0.01 max | 0.35max | Ni+Co 99 min | 0.40 max | 0.25max |
Mechanical properties
UNS | Tensile Strength Min,MPa | Yield Strength Min,KsiMPa | Elongation in 2 in or 50mm,Min,% |
UNS N02201 | 345 | 83 | 40 |
Available Size:OD: 6.35 ~ 219.1mm
WT:0.89 ~12 .7mm
L:20 Meter Max
Available Specifications:
ASTM B 161/ B 163/ B 751/ B775/ B 829
ASME SB 161/SB 163/SB 751/SB 775/ SB 829
Delivery Condition:
1: Annealed and Pickled
2: Bright and Annealed
3: Annealed and Pickled + Polishing
4: Bright Annealed+Polishing